NaCl溶液温度和含量对热处理后钢轨腐蚀行为的影响
李自立, 王欣纪, 田春洋, 叶沛聪, 刘海乔, 何成刚, 刘吉华

Influence of NaCl Temperature and Content on Corrosion Behavior of Heat Treated Rail Steel
LI Zili, WANG Xinji, TIAN Chunyang, YE Peicong, LIU Haiqiao, HE Chenggang, LIU Jihua
图6 热处理钢轨试样在不同NaCl溶液温度和腐蚀时间后的Nyquist和Bode图
Fig.6 Nyquist (a1-c1) and Bode (a2-c2) plots of heat-treated rail samples under different NaCl solution temperatures and different corrosion time: (a) 48 h, (b) 96 h, (c) 144 h