激光增材制造Ni-Cr-Mo合金在KCl-K2SO4 混合盐中的高温腐蚀行为研究 |
| 孔耀, 黄奕欣, 周木兰, 曾光, 宁华清, 申越, 刘宗德 |
|
High-temperature Corrosion Behavior of Laser Additive Manufacturing of Ni-Cr-Mo Alloy in KCl-K2SO4 Mixed Salt |
| KONG Yao, HUANG Yixin, ZHOU Mulan, ZENG Guang, NING Huaqing, SHEN Yue, LIU Zongde |
| 图6 TP347H不锈钢在600 ℃混合盐中腐蚀168 h后表面形貌 |
| Fig.6 Surface morphologies of different zones of TP347H stainless steel (a-c) after corrosion in mixed salts at 600 ℃ for 168 h |
|