一种低Re二代单晶高温合金的热腐蚀行为研究 |
| 杨鑫, 车欣, 卢玉章, 黄亚奇, 王栋, 申健 |
|
Hot Corrosion Behavior of a Low-Re Second-generation Single Crystal Superalloy |
| YANG Xin, CHE Xin, LU Yuzhang, HUANG Yaqi, WANG Dong, SHEN Jian |
| 图5 单一盐与混合盐环境镍基单晶高温合金在900 ℃热腐蚀20 h和100 h后的表面形貌图 |
| Fig.5 Surface morphologies of nickel-based single-crystal superalloy specimens corroded in pure salt (a, b, e, f) and mixed salt (c, d, g, h) after hot corrosion at 900°C for 20 h and 100 h |
|