海南滨海大气环境热浸镀锌钢室内外试验相关性分析
赵梓恒, 李波, 杨臻, 钱旺, 于浩, 张昊, 易盼, 陈俊航, 尹程辉, 肖葵

Correlation Analysis Between Indoor Test and Outdoor Test in Hainan Coastal Atmospheric Environment for Hot-dip Galvanized Steel
ZHAO Ziheng, LI Bo, YANG Zhen, QIAN Wang, YU Hao, ZHANG Hao, YI Pan, CHEN Junhang, YIN Chenghui, XIAO Kui
表3 热浸镀锌钢在海南滨海大气环境室内外试验后的腐蚀失重数据绝对差
Table 3 Absolute differences of corrosion mass loss data of hot-dip galvanized steel after indoor and outdoor tests in Hainan coastal atmospheric environment
Outdoor tests time / aIndoor tests time / cycD / μm
0.50.51.000
111.689
1.51.52.201
222.608
2.52.53.065