表2 热浸镀锌钢在海南滨海大气环境室内外试验后的腐蚀失重数据的初值化处理
Table 2 Initial processing of corrosion weight loss data of hot-dip galvanized steel after indoor and outdoor tests in Hainan coastal atmospheric environment
Outdoor testsIndoor tests
Time / aX0Time / cycXi
0.51.0000.51.000
11.78011.689
1.52.5501.52.201
23.31222.608
2.53.9502.53.065