静水压力对铸造与锻造Ti-6Al-4V合金应力腐蚀的影响差异研究
徐秋发, 郭岳, 刘骏, 杨东, 崔宇

Effect of Hydrostatic Pressure on Stress Corrosion Cracking of Cast and Forged Ti-6Al-4V Alloys
XU Qiufa, GUO Yue, LIU Jun, YANG Dong, CUI Yu
图12 Ti-6Al-4V合金在20 MPa静水压力下慢拉伸断口EBSD的KAM和GB结果
Fig.12 EBSD results of Ti-6Al-4V alloys slow tensile fracture under 20 MPa hydrostatic pressure: (a) kernel average misorientation (KAM) and (b) grain boundary (GB)