AH36船体钢在硫酸盐还原菌环境下的腐蚀机制研究
|
|
付磊, 张千, 林莉, 蹇科, 王雅君, 程飞, 彭东梅, 刘明
|
Corrosion Mechanism of AH36 Hull Steel in Sulfate-reducing Bacteria Environment
|
|
FU Lei, ZHANG Qian, LIN Li, JIAN Ke, WANG Yajun, CHENG Fei, PENG Dongmei, LIU Ming
|
|
表4 两种体系等效电路元件拟合参数
|
Table 4 Fitting parameters of equivalent circuit components of the two systems
|
|
| System | t / d | Rs / Ω·cm2 | Qf / F·cm-2 | nf | Rf / Ω·cm2 | Qdl / F·cm-2 | nd1 | Rct / Ω·cm2 |
|---|
| Sterile | 1 | 35.99 | 1.029 × 10-3 | 0.9954 | 1589 | 5.074 × 10-5 | 0.8061 | 5016 | | 3 | 40.57 | 1.298 × 10-3 | 0.9968 | 3598 | 9.982 × 10-5 | 0.7971 | 7408 | | 5 | 35.40 | 1.599 × 10-3 | 0.9587 | 5469 | 1.273 × 10-4 | 0.8137 | 9921 | | 10 | 35.10 | 1.359 × 10-3 | 0.9654 | 6982 | 1.276 × 10-4 | 0.8917 | 10310 | | 15 | 38.99 | 1.584 × 10-3 | 0.9854 | 6591 | 1.311 × 10-4 | 0.8765 | 13430 | | SRB | 1 | 30.92 | 3.428 × 10-3 | 0.8756 | 249.9 | 2.578 × 10-3 | 0.7894 | 964.4 | | 3 | 24.35 | 4.042 × 10-3 | 0.7865 | 145.7 | 6.124 × 10-3 | 0.7512 | 730.8 | | 5 | 25.72 | 3.385 × 10-3 | 0.7984 | 106.8 | 2.766 × 10-3 | 0.6574 | 684.7 | | 10 | 26.77 | 3.499 × 10-3 | 0.8169 | 136.6 | 2.932 × 10-3 | 0.8176 | 731.9 | | 15 | 26.65 | 3.305 × 10-3 | 0.7589 | 153.2 | 2.515 × 10-3 | 0.7456 | 814.6 |
|
|
|