AH36船体钢在硫酸盐还原菌环境下的腐蚀机制研究 |
| 付磊, 张千, 林莉, 蹇科, 王雅君, 程飞, 彭东梅, 刘明 |
|
Corrosion Mechanism of AH36 Hull Steel in Sulfate-reducing Bacteria Environment |
| FU Lei, ZHANG Qian, LIN Li, JIAN Ke, WANG Yajun, CHENG Fei, PENG Dongmei, LIU Ming |
| 图7 两种体系下不同腐蚀时间AH36钢基体表面形貌 |
| Fig.7 Surface morphologies of the AH36 steel substrate after 5 (a, d), 10 (b, e), 15 d (c, f) corrosion time under sterile solution (a-c) and SRB solution (d-f) |
|