含氧注气驱高Ca2+ 浓度工况下C110钢腐蚀产物膜演变及腐蚀行为研究 |
||||||||||||||||||||
| 赵密锋, 胡芳婷, 刘艳明, 宋文文, 谢俊峰, 吕祥鸿, 代盼, 胡航波 | ||||||||||||||||||||
|
Evolution of Corrosion Products Film and Corrosion Behavior of C110 Steel Under High-temperature and High-pressure O2-CO2 Atmosphere in a Simulated Drilling Fluid with High Mineral Content and High Concentration of Ca2+ |
||||||||||||||||||||
| ZHAO Mifeng, HU Fangting, LIU Yanming, SONG Wenwen, XIE Junfeng, LV Xianghong, DAI Pan, HU Hangbo | ||||||||||||||||||||
| 表1 高温高压腐蚀实验条件 |
||||||||||||||||||||
| Table 1 Test conditions of high temperature and high pressure corrosion experiments |
||||||||||||||||||||
|
||||||||||||||||||||