预充氢时间对不同显微组织无缝钢管钢高压氢脆敏感性影响
徐云峰, 程凯源, 黄峰, 杨宝齐, 程向龙, 昝启飞, 彭志贤, 刘静

Effect of Hydrogen Pre-charging Time on Hydrogen Embrittlement Susceptibility in High Pressure Hydrogen Environment for Two Seamless Steel Pipe Steels with Different Microstructures
XU Yunfeng, CHENG Kaiyuan, HUANG Feng, YANG Baoqi, CHENG Xianglong, ZAN Qifei, PENG Zhixian, LIU Jing
图11 10 MPa高压预充氢24 h后两种钢的裂纹结果:
Fig.11 SEM images (a1, b1), IPF maps (a2, b2) and KAM maps (a3, b3) of the X42QS (a1-a3) and X65 (b1-b3) steels after 24 h of pre-charging hydrogen at 10 MPa pressure