表3 电镀锡板样品在不同腐蚀溶液中浸泡后表面膜层的XPS分峰结果[31,34,35]
|
Table 3 Fitting results of the XPS spectra measured on tinplate after immersion in different corrosive solutions[31,34,35]
|
|
| Solutions | Peaks | Eb / eV | FWHM / eV | Peak areas | Chemical states | Related compounds |
|---|
| NaCl | Sn 3d5/2 | 486.4 | 1.56 | 143866 | Sn2+ | SnO/Sn(OH)2 | | pH ≈ 7.0 | | 486.9 | 1.25 | 74504.1 | Sn4+ | SnO2/Sn(OH)4 | | Cr 2p | 577.1 | 2.53 | 38350.2 | Cr3+ | Cr2O3/Cr(OH)3 | | | 586.8 | 2.45 | 16606.6 | Cr3+ | | O 1s | 530.4 | 2.02 | 89982.7 | O2- | SnO/SnO2/Cr2O3 | | | 531.6 | 1.73 | 116474.9 | OH- | Sn(OH)2/Sn(OH)4/Cr(OH)3 | | | 532.8 | 2.13 | 50950.3 | Bound water | | | NaCl + NaSO3 | Sn 3d5/2 | 485.0 | 1.69 | 45486.9 | Sn0 | Metallic Sn | | pH ≈ 4.0 | | 486.5 | 1.59 | 120150.4 | Sn2+ | SnO/Sn(OH)2 | | | 487.1 | 1.47 | 94504.8 | Sn4+ | SnO2/Sn(OH)4 | | Cr 2p | 577.3 | 2.56 | 79160.8 | Cr3+ | Cr2O3/Cr(OH)3 | | | 587.0 | 2.46 | 37673.3 | Cr3+ | | O 1s | 530.5 | 2.06 | 80480.9 | O2- | SnO/SnO2/Cr2O3 | | | 531.7 | 1.75 | 176386.6 | OH- | Sn(OH)2/Sn(OH)4/Cr(OH)3 | | | 532.8 | 2.18 | 59167.1 | Bound water | |
|
|
|