电镀锡板表面Cr2O3 钝化膜结构及耐蚀性演化的电化学阻抗谱研究
|
|
刘状, 乔创, 姜金利, 车欣, 代春丽, 沈勇, 郝龙
|
Structure- and Corrosion Resistance-evolution of Cr2O3 Passivation Film on Tinplate Surface in Neutral NaCl- and Acidic NaCl + Na2SO3-solution
|
|
LIU Zhuang, QIAO Chuang, JIANG Jinli, CHE Xin, DAI Chunli, SHEN Yong, HAO Long
|
|
表1 拟合图3a中EIS数据得到的电化学参数
|
Table 1 Electrical parameters obtained from fitting the EIS data in Fig.3a1 and a2
|
|
| Immersion time / h | Rs / Ω·cm2 | Qo / 10-6 F·cm-2 | no | Ro / Ω·cm2 | Qi / 10-6 F·cm-2 | ni | Ri / 105 Ω·cm2 | χ2 / 10-4 |
|---|
| 0 | 7.972 | 5.096 | 0.819 | 1971 | 5.296 | 0.895 | 12.060 | 16.2 | | 1 | 7.868 | 6.459 | 0.810 | 1497 | 5.429 | 0.901 | 10.792 | 12.7 | | 2 | 7.790 | 7.004 | 0.806 | 1303 | 5.470 | 0.903 | 9.081 | 11.6 | | 3 | 7.752 | 7.010 | 0.807 | 1279 | 5.339 | 0.907 | 7.380 | 16.1 | | 4 | 7.679 | 7.361 | 0.801 | 1227 | 5.553 | 0.912 | 5.822 | 15.4 | | 5 | 7.662 | 7.669 | 0.801 | 1246 | 5.733 | 0.907 | 5.891 | 13.6 | | 6 | 7.644 | 8.057 | 0.798 | 1192 | 5.705 | 0.907 | 5.952 | 11.7 | | 7 | 7.677 | 8.329 | 0.797 | 1085 | 5.693 | 0.904 | 6.694 | 10.2 | | 8 | 7.659 | 9.167 | 0.789 | 996 | 5.526 | 0.911 | 9.354 | 12.5 | | 9 | 7.701 | 9.475 | 0.789 | 919 | 5.577 | 0.908 | 12.110 | 12.8 | | 10 | 7.732 | 9.637 | 0.788 | 927.9 | 5.482 | 0.913 | 20.160 | 10.8 |
|
|
|