Q345R碳钢在Hitec高温熔盐中动态腐蚀特性实验对比研究 |
| 魏旭光, 王维斌, 李康, 张灿灿, 吴玉庭, 鹿院卫, 王国强, 赵博 |
|
Dynamic Corrosion Behavior of Q345R Carbon Steel in High-temperature Hitec Molten Salt |
| WEI Xuguang, WANG Weibin, LI Kang, ZHANG Cancan, WU Yuting, LU Yuanwei, WANG Guoqiang, ZHAO Bo |
| 图6 Q345R碳钢在400 ℃下流速为0和2 m/s Hitec熔盐中腐蚀1000 h后横截面的EDS映射图 |
| Fig.6 EDS mappings of the cross-section of a Q345R carbon steel after corrosion in Hitec molten salt at 400 ℃ for 1000 h with 0 m/s (a) and 2 m/s (b) |
|