混凝土配重层对近海海底钢质管道阴极保护效果的影响
王萌萌, 曹国民, 孟繁兴, 李天亮, 宋沁峰, 单太航, 董亮

Influence of Concrete Counterweight Layer on Cathodic Protection Effect of Nearshore Submarine Steel Pipes
WANG Mengmeng, CAO Guomin, MENG Fanxing, LI Tianliang, SONG Qinfeng, SHAN Taihang, DONG Liang
表3 在静态海水和海泥中带混凝土层X60钢稳态极化数据
Table 3 Steady-state polarization data of concrete weighted X60 steel in static environment
5‰ salinity seawater16.8‰ salinity seawater26.7‰ salinity seawaterSea mud
Ep, CSE / mVI / mA·m-2Ep, CSE / mVI / mA·m-2Ep, CSE / mVI / mA·m-2Ep, CSE / mVI / mA·m-2
-5740-5910-6040-5620
-86723.428-83442.341-86856.427-82916.338
-94526.204-88073.960-94777.533-89618.221
-101136.321-978103.107-1019169.121-101024.073
-106852.883-1076173.679-1081228.427-108134.603
-112075.333-1151239.587-1149316.116-110450.578
-1154102.461-1201311.849-1221396.476-116791.378