寒带海洋环境下金属材料腐蚀与防护研究进展
|
|
李亮, 殷文昌, 郜阿旺, 韩小乐, 杨延格
|
Research Progress on Corrosion and Protection of Metallic Materials in Polar Marine Environments
|
|
LI Liang, YIN Wenchang, GAO Awang, HAN Xiaole, YANG Yange
|
|
表1 金属材料在寒带大气环境中的腐蚀速率[21,22]
|
Table 1 Corrosion rates of metals in polar atmospheric environments[21,22]
|
|
| Material | Exposure site | Test period / a | Corrosion rate / μm·a-1 |
|---|
| Mild steel | Jubany base | 1 | 38.1 | | Marsh base | 1 | 24.1 | | Artigas base | 1 | 65.8 | | Steel St3 | Mirnyi station | 1 | 7.8 | | Q235 | Zhongshan station | 1 | 16.3 | | Q460 | Zhongshan station | 1 | 10.8 | | Q960 | Zhongshan station | 1 | 15.8 | | Ni-Cr-Mo-V steel | Zhongshan station | 1 | 13.0 | | Aluminium | Jubany base | 1 | 4.03 | | Marsh base | 1 | 3.65 | | Artigas base | 1 | 2.49 | | Copper | Jubany base | 1 | 2.03 | | Artigas base | 1 | 2.16 | | Mirnyi station | 1 | 1.1 | | Zinc | Jubany base | 1 | 1.89 | | Artigas base | 1 | 2.11 |
|
|
|