铜封端负载8-HQ埃洛石纳米管镁合金微弧氧化自修复涂层的制备及耐蚀性能
施艳1, 饶智航1, 缪程平1, 张洋1, 陈赵扬2, 屠晓华1(), 李加友1, 褚有群2()
Preparation and Corrosion Resistance of a Copper-capped 8-HQ-loaded Halloysite Nanotube-based Self-healing Coating on Mg-alloy via Micro-arc Oxidation
SHI Yan1, RAO Zhihang1, MIAO Chengping1, ZHANG Yang1, CHEN Zhaoyang2, TU Xiaohua1(), LI Jiayou1, CHU Youqun2()

图7. 4种MAO涂层在3.5%NaCl溶液中的开路电位-时间变化曲线。

Fig.7. OCP curves of MAO, HNTs-MAO, 8-HQ-HNTs-MAO and Cu-8-HQ-HNTs-MAO coatings immersed in 3.5%NaCl solution for 1 (a), 3 (b), 5 (c), 7 (d), 8 (e), 9 (f), 24 (g) and 168 h (h)