高温蒸汽环境下K444和K452合金及涂层的氧化行为
张超, 何闯, 夏凯, 郭亭山, 梁志远

Oxidation Behavior of K444 and K452 Alloys with and Without Thermal Barrier Coatings in High- temperature Steam Environment
ZHANG Chao, HE Chuang, XIA Kai, GUO Tingshan, LIANG Zhiyuan
表4 K452合金氧化100、200和300 h后氧化产物表面EDS元素分析结果 (mass fraction / %)
Table 4 EDS elements analysis results of corrosion surfaces of K452 alloy after 100, 200 and 300 h in Fig.5
PointsCrNiNbMoAlTiCoW
12.554.20.10.10.121.10.11.1
29.078.3--0.10.2-0.1
34.770.20.10.10.15.50.10.4
413.872.70.1-0.11.80.10.2
56.475.40.1-0.40.60.20.1
628.361.10.10.10.12.30.10.1