[an error occurred while processing this directive]
高温蒸汽环境下K444和K452合金及涂层的氧化行为
张超1,2, 何闯3, 夏凯1, 郭亭山3, 梁志远3()
Oxidation Behavior of K444 and K452 Alloys with and Without Thermal Barrier Coatings in High- temperature Steam Environment
ZHANG Chao1,2, HE Chuang3, XIA Kai1, GUO Tingshan3, LIANG Zhiyuan3()

图9. 1000 ℃下Ni-Cr-Ti-H-O体系的热力学相图

Fig.9. Thermodynamic phase diagram of the Ni-Cr-Ti-H-O system at 1000 ℃: (a) Ni-Cr-Al-H-O, (b) Ni-Cr-Ti-H-O