高温蒸汽环境下K444K452合金及涂层的氧化行为
张超1,2, 何闯3, 夏凯1, 郭亭山3, 梁志远3()
Oxidation Behavior of K444 and K452 Alloys with and Without Thermal Barrier Coatings in High- temperature Steam Environment
ZHANG Chao1,2, HE Chuang3, XIA Kai1, GUO Tingshan3, LIANG Zhiyuan3()

图3. K444、K452合金和涂层材料分别氧化100、200 和300 h后的XRD谱

Fig.3. XRD patterns of alloys without and with coatings after steam oxidation for 100, 200 and 300 h: (a) K444 alloy, (b) K452 alloy, (c) PtAl + YSZ coating, (d) CoCrAlY + YSZ coating