(Ni, Pt)Al和NiCoCrAlYTa涂层对镍基单晶高温合金DD6抗热腐蚀性能的影响
|
|
Hot Corrosion Resistance of (Ni, Pt)Al- and NiCoCrAlYTa-coating Prepared on Ni-based Single Crystal Alloy DD6
|
|
图9. 两种涂层在900 ℃下热腐蚀200 h和300 h后的XRD图谱 |
Fig.9. XRD patterns of (Ni, Pt)Al coating (a, b) and NiCoCrAlYTa coating (c, d) after hot corrosion in Na2SO4 + 5%NaCl mixed salt at 900 ℃ for 200 h (a, c) and 300 h (b, d) |
![]() |