再生镁合金表面微弧氧化/水滑石复合膜层的一步法制备及其耐蚀性能研究
张云, 张宇鹏, 董泽华, 张欣欣

One-step Preparation and Corrosion Performance of Micro-arc Oxidation/hydrotalcite Composite Film on Recycled Mg-alloys
ZHANG Yun, ZHANG Yupeng, DONG Zehua, ZHANG Xinxin
表2 Recycled Mg-MAO和Recycled Mg-MAO/LDH的EIS拟合结果
Table 2 EIS fitting results of recycled Mg-MAO and recycled Mg-MAO/LDH
SampleRs / Ω·cm2Qf / F·cm-2nfRf / Ω·cm2Qdl / F·cm-2ndlRct / Ω·cm2Rp / Ω·cm2
Mg-MAO12.217.1 × 10-80.815641.7 × 10-50.511629016854
Mg-MAO/LDH12.653.2 × 10-70.7222792.7 × 10-60.651845020729