Al-10%RE (RE = Ce、Nd、Y、La)合金在典型海洋大气环境下的腐蚀行为研究
谢睿1,2,3,4, 蒋全通1,2,3,4(), 韩东晓5, 陈烨5, 刘万鹏5, 裴炎彤5, 段继周1,2,3,4, 侯保荣1,2,3,4
Corrosion Behavior of Al-10%RE (RE = Ce, Nd, Y, La) Alloys in Typical Marine Atmospheric Environments
XIE Rui1,2,3,4, JIANG Quantong1,2,3,4(), HAN Dongxiao5, CHEN Ye5, LIU Wanpeng5, PEI Yantong5, DUAN Jizhou1,2,3,4, HOU Baorong1,2,3,4

图14. Al-RE合金在大气暴露过程中的腐蚀机理示意图

Fig.14. Schematic diagrams of corrosion mechanisms of Al-RE alloys during atmospheric exposure at Qingdao station (a-c) and Sanya station (a, b, d)