Al-10%RE (RE = Ce、Nd、Y、La)合金在典型海洋大气环境下的腐蚀行为研究
谢睿1,2,3,4, 蒋全通1,2,3,4(), 韩东晓5, 陈烨5, 刘万鹏5, 裴炎彤5, 段继周1,2,3,4, 侯保荣1,2,3,4
Corrosion Behavior of Al-10%RE (RE = Ce, Nd, Y, La) Alloys in Typical Marine Atmospheric Environments
XIE Rui1,2,3,4, JIANG Quantong1,2,3,4(), HAN Dongxiao5, CHEN Ye5, LIU Wanpeng5, PEI Yantong5, DUAN Jizhou1,2,3,4, HOU Baorong1,2,3,4

图13. 在三亚和青岛站大气暴晒110 d后的Al-10%RE合金在天然海水中极化曲线测试结果

Fig.13. Polarization curves of Al-10%RE alloys exposed at Sanya station (a) and Qingdao station (b) in natural seawater