[an error occurred while processing this directive]
海上光伏关键结构的腐蚀与防护综述
陈晓华1, 满成1, 甄永泰2, 付龙3, 崔洪芝1()
Review on Corrosion and Protection of Key Structures for Offshore Photovoltaic Industry
CHEN Xiaohua1, MAN Cheng1, ZHEN Yongtai2, FU Long3, CUI Hongzhi1()

图4. 中性盐雾条件下镀锌钢腐蚀不同时间的宏观形貌[43]

Fig.4. Corrosion macroscopic photos of galvanized steel at 0 h (a), 1000 h (b), 1500 h (c), 3000 h (d), 4000 h (e) and 5000 h (f) under neutral salt spray conditions of 0 μm (a1-f1), 65 μm (a2-f2), 85 μm (a3-f3) and 100 μm (a4-f4) coating[43]