热处理工艺对增材制造金属零件腐蚀行为影响的研究进展
周丽, 曹晓蝶, 来佑彬, 丁旺旺, 韦博鑫, 吴嘉俊

Research Progress in Influence of Heat Treatment on Corrosion Behavior of Additive Manufactured Parts
ZHOU Li, CAO Xiaodie, LAI Youbin, DING Wangwang, WEI Boxin, WU Jiajun
图10 LPBF-316L样品在室温下在3.5%NaCl溶液中进行动电位极化测试后表面微观形貌[55]
Fig.10 Optical microscopy images (a, b, g, h) and SEM images (c-f, i, j) of LPBF-316L As-built samples (a-f), HIP-treated samples (g, h)[55] after potentiodynamic polarization testing in 3.5%NaCl solution at room temperature