乙二醇-水冷媒中Cu-Al电偶腐蚀行为及反应机制研究
陈思敏, 练龙江, 黄延淞, 曾兰香, 雷冰, 孟国哲

Galvanic Corrosion Behavior and Reaction Mechanism of Cu-Al Couple in Ethylene Glycol-Water Coolent
CHEN Simin, LIAN Longjiang, HUANG Yansong, ZENG Lanxiang, LEI Bing, MENG Guozhe
表5 依据点蚀坑密度和大小对点蚀等级评定[32]
Table 5 Grade evaluation of pitting based on pit density and pit size[32]
Corrosion gradeABC
Density / points·m-2Size / mm2Depth / mm
1≤ 2.5 × 103≤ 0.5≤ 0.4
22.5 × 103-1 × 1040.5-2.00.4-0.8
31 × 104-5 × 1042.0-8.00.8-1.6
45 × 104-1 × 1058.0-12.51.6-3.2
51 × 105-5 × 10512.5-24.53.2-6.4