δ-铁素体对增材制造304L不锈钢液态铅铋腐蚀行为的影响
庞曰艺, 张立波, 宁方强, 赵志坡, 闫宏, 刘佳

Effect of δ-ferrite on Corrosion Behavior of Additively Manufactured 304L Stainless Steel in Liquid Lead-bismuth
PANG Yueyi, ZHANG Libo, NING Fangqiang, ZHAO Zhipo, YAN Hong, LIU Jia
图7 WAAM 304L不锈钢在550 ℃、贫氧的液态LBE中浸泡1000 h下δ-铁素体的SEM形貌图
Fig.7 SEM morphologies of δ-ferrite of WAAM 304L stainless steel after 1000 h exposed in liquid LBE under poor-oxygen condition at 550 oC: (a) low morphology, (b-d) high morphology