SLM-316L不锈钢的高温氧化与腐蚀行为研究 |
| 冯浩轩, 王馥丽, 李甲林, 杜瑶, 韦博鑫, 朱圣龙 |
|
High Temperature Oxidation and Corrosion Behavior of 316L Stainless Steel Prepared by Selected Laser Melting Process |
| FENG Haoxuan, WANG Fuli, LI Jialin, DU Yao, WEI Boxin, ZHU Shenglong |
| 图8 Cast-316与SLM-316不锈钢试样在沉积固态NaCl、700 ℃环境下的腐蚀200 h后试样的表面形貌 |
| Fig.8 Surface morphologies of Cast-316 (a, b) and SLM-316 (c, d) stainless steels after corrosion for 200 h at 700 oC with solid NaCl deposited |
|