SLM-316L不锈钢的高温氧化与腐蚀行为研究
冯浩轩, 王馥丽, 李甲林, 杜瑶, 韦博鑫, 朱圣龙

High Temperature Oxidation and Corrosion Behavior of 316L Stainless Steel Prepared by Selected Laser Melting Process
FENG Haoxuan, WANG Fuli, LI Jialin, DU Yao, WEI Boxin, ZHU Shenglong
图7 Cast-316与SLM-316不锈钢试样在700 ℃、沉积固态NaCl环境下腐蚀200 h后的XRD谱图
Fig.7 XRD patterns of Cast-316 and SLM-316 stainless steels after corrosion for 200 h at 700 oC with solid NaCl deposited