SLM-316L不锈钢的高温氧化与腐蚀行为研究 |
| 冯浩轩, 王馥丽, 李甲林, 杜瑶, 韦博鑫, 朱圣龙 |
|
High Temperature Oxidation and Corrosion Behavior of 316L Stainless Steel Prepared by Selected Laser Melting Process |
| FENG Haoxuan, WANG Fuli, LI Jialin, DU Yao, WEI Boxin, ZHU Shenglong |
| 图4 Cast-316与SLM-316在700 ℃下氧化200 h后的微观表面、截面形貌 |
| Fig.4 Surface and cross-sectional morphologies of Cast-316 (a-c) and SLM-316 (d-f) stainless steels after oxidation for 200 h at 700 oC |
|