激光定向能量沉积17-4PH不锈钢钝化与点蚀行为研究
谷清宇, 宋雁飞, 张亮亮, 王楠, 雷晓维

Passivation and Pitting Corrosion Behavior of Laser Directed Energy Deposited 17-4PH Stainless Steel
GU Qingyu, SONG Yanfei, ZHANG Liangliang, WANG Nan, LEI Xiaowei
图8 17-4PH不锈钢在6%FeCl3溶液中浸泡8 h后的点蚀形貌
Fig.8 Pitting morphologies of 17-4PH stainless steel after immersion corrosion in 6%FeCl3 solution for 8 h: (a, b) extruded sample, (c, d) 2#DED sample