新型耐微生物腐蚀油管钢的硫酸盐还原菌腐蚀行为研究
杨宝齐, 闫茂成, 史显波, 高博文

SRB Induced Corrosion Behavior of a Novel Microbial Corrosion Resistant Pipeline Steel
YANG Baoqi, YAN Maocheng, SHI Xianbo, GAO Bowen
表3 接菌培养基中的EIS拟合结果
Table 3 Fitting results of EIS of two test steels in Fig.8
SamplesTime / dRs / Ω·cm2Rbc / Ω·cm2Qbc / Ω-1·cm-2·s nRct / Ω·cm2Qct / Ω-1·cm-2·s n
Ordinary steel13.6480085.82 × 10-452.971.43 × 10-3
23.5291033.12 × 10-30.2581.73 × 10-2
43.6133113.79 × 10-34831.20 × 10-2
73.8746716.44 × 10-329304.01 × 10-3
103.8120456.39 × 10-331144.87 × 10-3
143.8710196.34 × 10-373396.29 × 10-3
MIC resistant steel13.560.115.09 × 10-42.31×1046.01 × 10-4
23.626922.02 × 10-327.916.14 × 10-3
43.4724.51.02 × 10-22693.70 × 10-3
73.558.263.71 × 10-31.66 × 1042.83 × 10-3
103.5938.23.23 × 10-31.37 × 1042.93 × 10-3
143.6536.33.52 × 10-35.66 × 1042.10 × 10-3