表2 7075-X70耦合试样在未含和含有200 mg/L SIP的3.5%NaCl溶液中浸泡24 h后阻抗谱拟合参数
Table 2 Fitting parameters of Nyquist diagrams of 7075-X70 coupling specimen immersed for 24 h in 3.5%NaCl solutions without and with 200 mg/L SIP
SloutionRs / Ω·cm2Y0Qf / Ω-1·cm-2·snRf / Ω·cm2Y0Qdl / Ω-1·cm-2·s nnRct / Ω·cm2
Without SIP7.1192.825 × 10-50.8925401.431 × 10-30.99853.3
With SIP6.9282.7 × 10-50.9132414.67 × 10-40.937485