316L不锈钢焊接接头在含S-H2S环境中的腐蚀行为
李科, 李天雷, 曹晓燕, 姜流, 王雅熙, 肖泽渝, 钟显康

Corrosion Behavior of 316L Stainless Steel Welded Joints in S-H2S-containing Environments
LI Ke, LI Tianlei, CAO Xiaoyan, JIANG Liu, WANG Yaxi, XIAO Zeyu, ZHONG Xiankang
表2 316L不锈钢焊缝、母材以及热影响区试样在不同实验条件下的局部腐蚀速率 (mm/a)
Table 2 Localized corrosion rates of WS, BM and HAZ of 316L stainless steel under different experimental conditions
Temperature oCWelded seamBase materialHeat affected zone
90125.59590.297124.291
12086.59042.75760.861