316L不锈钢焊接接头在含S-H2S环境中的腐蚀行为
李科, 李天雷, 曹晓燕, 姜流, 王雅熙, 肖泽渝, 钟显康

Corrosion Behavior of 316L Stainless Steel Welded Joints in S-H2S-containing Environments
LI Ke, LI Tianlei, CAO Xiaoyan, JIANG Liu, WANG Yaxi, XIAO Zeyu, ZHONG Xiankang
图3 316L不锈钢WS、BM以及HAZ试样在不同实验条件下的XPS精细谱
Fig.3 XPS fine spectra of Fe 2p (a, b), S 2p (c, d) and Cr 2p (e, f) for WS, BM and HAZ of 316L stainless steel after corrosion under 90 oC, pH = 3.5, 1 MPa H2S, 1000 mg/L Cl- (a, c, e) and 120 oC, pH = 3.5, 0.1 MPa H2S, 1000 mg/L Cl- (b, d, f)