316L不锈钢焊接接头在含S-H2S环境中的腐蚀行为 |
| 李科, 李天雷, 曹晓燕, 姜流, 王雅熙, 肖泽渝, 钟显康 |
|
Corrosion Behavior of 316L Stainless Steel Welded Joints in S-H2S-containing Environments |
| LI Ke, LI Tianlei, CAO Xiaoyan, JIANG Liu, WANG Yaxi, XIAO Zeyu, ZHONG Xiankang |
| 图2 316L不锈钢WS、BM以及HAZ试样在不同条件腐蚀试验后的3D形貌 |
| Fig.2 3D surface morphologies of WS (a, b), BM (c, d) and HAZ (e, f) of 316L stainless steel after corrosion under 90 oC, pH = 3.5, 1 MPa H2S, 1000 mg/L Cl- (a, c, e) and 120 oC, pH = 3.5, 0.1 MPa H2S, 1000 mg/L Cl- (b, d, f) |
|