NaCl347HGH3539在熔融硝酸盐中热腐蚀行为的影响
彭望, 陈荐, 杨凌旭, 刘会军, 梁建平, 曾潮流

Effect of NaCl on Hot Corrosion Behavior of 347H Stainless Steel and Ni-based GH3539 Alloy in Molten Nitrate Salts
PENG Wang, CHEN Jian, YANG Lingxu, LIU Huijun, LIANG Jianping, ZENG Chaoliu
图10 GH3539合金在600 ℃熔融(Na, K)NO3-5%NaCl热腐蚀100 h和400 h后的断面形貌
Fig.10 Cross-sectional morphologies of GH3539 alloy after hot corrosion in molten (Na, K)NO3-5%NaCl at 600 oC for 100 h (a, b) and 400 h (c, d)