液相氟化处理Ti45Al8.5Nb合金高温氧化行为研究
庄钊涛, 严豪杰, 谢冰, 桂也, 孙擎擎, 伍廉奎, 曹发和

High-temperature Oxidation Behavior of Liquid-phase Fluorination Treated Ti45Al8.5Nb Alloy
ZHUANG Zhaotao, YAN Haojie, XIE Bing, GUI Ye, SUN Qingqing, WU Liankui, CAO Fahe
图2 Ti45Al8.5Nb合金在无水及含1%,3%和5%水的NH4F乙二醇溶液中液相处理后表面形貌
Fig.2 Surface morphologies of Ti45Al8.5Nb alloy after liquid-phase fluorination in NH₄F-ethylene glycol solutions containing 0% (a), 1% (b), 3% (c) and 5% (d) H2O