碳点缓蚀剂的研究进展及展望 |
| 陈宇, 魏高飞, 邓书端, 李向红 |
|
Research Progress and Prospects of Carbon Dots as Corrosion Inhibitors |
| CHEN Yu, WEI Gaofei, DENG Shuduan, LI Xianghong |
| 图11 Q235电极分别在不同浓度的HCl、NaCl溶液中浸泡24 h后的电流密度分布图和EIS图[ |
| Fig.11 Current density distribution diagrams and EIS diagrams of Q235 electrodes after being soaked in HCl and NaCl solutions with different concentrations for 24 h: (a) HCl-0 mg/L-24 h, (b) HCl-25 mg/L-24 h, (c) HCl-200 mg/L-24 h, (d) NaCl-0 mg/L-24 h, (e) NaCl-25 mg/L-24 h, (f) NaCl-200 mg/L-24 h, and EIS of Q235 steel after immersing in HCl (a1-c1) and NaCl (d1-f1) for 24 h[ |
|