CO2-CO气氛下3.5%硅钢固态脱碳氧化层演变规律
孙伶艳, 洪陆阔, 孙彩娇, 艾立群, 周美洁, 闻莉

Evolution of Oxide Scale of 3.5% Silicon Steel in Solid State Decarburization in CO2-CO Atmospheres
SUN Lingyan, HONG Lukuo, SUN Caijiao, AI Liqun, ZHOU Meijie, WEN Li
图7 两种气体流量下脱碳30 min后硅钢表面氧化层截面形貌
Fig.7 Cross-sectional morphologies of 3.5% silicon steel after decarburization for 30 min at the gas flow rates of 450 mL·min-1 (a) and 850 mL·min-1 (b)