CO2-CO气氛下3.5%硅钢固态脱碳氧化层演变规律
孙伶艳, 洪陆阔, 孙彩娇, 艾立群, 周美洁, 闻莉

Evolution of Oxide Scale of 3.5% Silicon Steel in Solid State Decarburization in CO2-CO Atmospheres
SUN Lingyan, HONG Lukuo, SUN Caijiao, AI Liqun, ZHOU Meijie, WEN Li
图3 在2种PCO2/PCO条件下脱碳后硅钢表面氧化层的截面形貌对比
Fig.3 Cross sections of oxide scales formed on 3.5% silicon steel during decarbonization under different conditions: (a) PCO2/PCO = 0.10, (b) PCO2/PCO = 0.30