Cu-15Ni-8Sn合金在含S2-3.5%NaCl溶液中的腐蚀行为
范世林, 杜娟, 杨少丹, 周延军, 宋克兴, 张国赏, 岳鹏飞, 杨冉, 王晓军

Corrosion Behavior of Cu-15Ni-8Sn Alloy in 3.5%NaCl Solution Containing S2-
FAN Shilin, DU Juan, YANG Shaodan, ZHOU Yanjun, SONG Kexing, ZHANG Guoshang, YUE Pengfei, YANG Ran, WANG Xiaojun
图5 Cu-15Ni-8Sn合金在不同含量Na2S的3.5%NaCl溶液中浸泡30 d的截面形貌和元素分布
Fig.5 Cross-sectional morphologies and element distributions of Cu-15Ni-8Sn alloy after 30 d immersion in 3.5%NaCl solutions containing 0 mg/L (a) and 10 mg/L (b) Na2S