Cu-15Ni-8Sn合金在含S2-3.5%NaCl溶液中的腐蚀行为
范世林, 杜娟, 杨少丹, 周延军, 宋克兴, 张国赏, 岳鹏飞, 杨冉, 王晓军

Corrosion Behavior of Cu-15Ni-8Sn Alloy in 3.5%NaCl Solution Containing S2-
FAN Shilin, DU Juan, YANG Shaodan, ZHOU Yanjun, SONG Kexing, ZHANG Guoshang, YUE Pengfei, YANG Ran, WANG Xiaojun
图4 Cu-15Ni-8Sn合金浸泡在Na2S含量不同的3.5%NaCl溶液中浸泡不同时间后的表面微观形貌与成分
Fig.4 Surface micro-morphologies and elemental contents of Cu-15Ni-8Sn alloy after immersion in 3.5%NaCl solutions containing 0 mg/L (a-d) and 10 mg/L (e-h) Na2S for 1 d (a, e), 6 d (b, f), 18 d (c, g) and 30 d (d, h)