Cu-15Ni-8Sn合金在含S2- 的3.5%NaCl溶液中的腐蚀行为 |
| 范世林, 杜娟, 杨少丹, 周延军, 宋克兴, 张国赏, 岳鹏飞, 杨冉, 王晓军 |
|
Corrosion Behavior of Cu-15Ni-8Sn Alloy in 3.5%NaCl Solution Containing S2- |
| FAN Shilin, DU Juan, YANG Shaodan, ZHOU Yanjun, SONG Kexing, ZHANG Guoshang, YUE Pengfei, YANG Ran, WANG Xiaojun |
| 图2 Cu-15Ni-8Sn合金在含不同浓度Na2S的3.5NaCl溶液中浸泡30 d内的Nyquist图及Bode图 |
| Fig.2 Nyquist plots (a, d) and Bode plots (b, c, e, f) of Cu-15Ni-8Sn alloy after immersion for different time in 3.5%NaCl solutions containing 0 mg/L (a-c) and 10 mg/L (d-f) Na2S |
|