不同温度下DD10合金钎焊接头热腐蚀行为研究 |
| 赵欣宇, 刘恩泽, 张功, 赵媛, 宁礼奎, 信昕, 贾丹, 刘伟华, 谭政 |
|
Hot Corrosion Behavior of Brazed Joints of Single Crystal Ni-based DD10 Alloy Beneath Na2SO4 Deposit in Air at 850 and 900 ℃ |
| ZHAO Xinyu, LIU Enze, ZHANG Gong, ZHAO Yuan, NING Likui, XIN Xin, JIA Dan, LIU Weihua, TAN Zheng |
| 图6 DD10合金在850 ℃下200 h热腐蚀后的截面SEM形貌及EDS元素面扫描 |
| Fig.6 Cross-section SEM morphology and corresponding EDS mapping results of DD10 alloy after hot corrosion at 850 ℃ for 200 h |
|