钛基体阴极充氢处理对RuO2-IrO2-TiO2 阳极微观结构和性能的影响
刘鹏鹤, 薛丽莉, 许立坤, 辛永磊, 郭明帅, 周帅, 段体岗

Effect of Hydrogen Pre-charging for Ti-substrate on Microstructure and Electrochemical Properties of Ti/RuO2-IrO2-TiO2 Anode
LIU Penghe, XUE Lili, XU Likun, XIN Yonglei, GUO Mingshuai, ZHOU Shuai, DUAN Tigang
表4 钛基体未充氢和经不同电流密度充氢后制备的氧化物阳极的双电层电容和形貌因子
Table 4 Double-layer capacitances and morphological factors of the oxide anodes on titanium substrates uncharged and charged with hydrogen at different current densities
I / mA·cm-2Cdl / μF·cm-2φ
Uncharged5.310.133
505.750.144
1007.970.199
2508.270.207
5008.050.201