钛基体阴极充氢处理对RuO2-IrO2-TiO2 阳极微观结构和性能的影响
刘鹏鹤, 薛丽莉, 许立坤, 辛永磊, 郭明帅, 周帅, 段体岗

Effect of Hydrogen Pre-charging for Ti-substrate on Microstructure and Electrochemical Properties of Ti/RuO2-IrO2-TiO2 Anode
LIU Penghe, XUE Lili, XU Likun, XIN Yonglei, GUO Mingshuai, ZHOU Shuai, DUAN Tigang
表2 钛基体未充氢和经不同电流密度充氢后制备的氧化物阳极的EIS拟合参数
Table 2 Fitting parameters of EIS of the oxide anodes on titanium substrates uncharged and charged with hydrogen at different current densities
I / mA·cm-2Rs / Ω·cm2Qdl / mΩ·cm2·SnnRct / Ω·cm2W / Ω·cm2
Uncharged32.979.250.7912.573.37
5031.0510.50.8110.251.84
10029.7710.90.807.152.20
25031.3619.30.744.041.49
50031.1615.00.774.341.51