高压凝固Mg-xAl (x = 3, 5, 7, 9, 12)合金组织结构及耐腐蚀性能
郭耀威, 艾士民, 房大然, 林小娉, 杨连威, 郑哲皓

Microstructure and Corrosion Resistance of High-pressure Solidified Mg-xAl (x = 3, 5, 7, 9, 12) Alloys
GUO Yaowei, AI Shimin, FANG Daran, LIN Xiaoping, YANG Lianwei, ZHENG Zhehao
图15 常规铸造及高压凝固Mg-xAl合金在3.5%NaCl溶液中浸泡24 h的XPS光谱
Fig.15 XPS spectra of conventional cast Mg-5Al (a1-a3) and high-pressure solidified Mg-5Al (b1-b3) and Mg-9Al (c1-c3) alloys soaked in 3.5%NaCl solution for 24 h