高压凝固Mg-xAl (x = 3, 5, 7, 9, 12)合金组织结构及耐腐蚀性能
郭耀威, 艾士民, 房大然, 林小娉, 杨连威, 郑哲皓

Microstructure and Corrosion Resistance of High-pressure Solidified Mg-xAl (x = 3, 5, 7, 9, 12) Alloys
GUO Yaowei, AI Shimin, FANG Daran, LIN Xiaoping, YANG Lianwei, ZHENG Zhehao
图13 高压凝固Mg-Al合金在3.5%NaCl水溶液中浸泡2 h后的SEM腐蚀形貌
Fig.13 SEM corrosion morphologies of high-pressure solidified Mg-xAl alloys after immersion in 3.5%NaCl solution for 2 h: (a) Mg-3Al, (b) Mg-5Al, (c) Mg-7Al, (d) Mg-9Al, (e, f) Mg-12Al