高压凝固Mg-xAl (x = 3, 5, 7, 9, 12)合金组织结构及耐腐蚀性能 |
| 郭耀威, 艾士民, 房大然, 林小娉, 杨连威, 郑哲皓 |
|
Microstructure and Corrosion Resistance of High-pressure Solidified Mg-xAl (x = 3, 5, 7, 9, 12) Alloys |
| GUO Yaowei, AI Shimin, FANG Daran, LIN Xiaoping, YANG Lianwei, ZHENG Zhehao |
| 图7 常规铸造和高压凝固Mg-xAl (x = 3,5,7,9,12)合金的Nyquist图 |
| Fig.7 Nyquist plots of conventional cast Mg-3Al, Mg-5Al and Mg-7Al alloys (a), Mg-9Al and Mg-12Al alloys (b), and high-pressure (4 GPa) solidified Mg-xAl (x = 3, 5, 7, 9, 12) alloys (c) |
|